Lateral stiffness testing on H.S.T. clouth rubber primary spring (TM-DOS-017)

Last updated on 02 August 2013 2:52
1. The springs were found to have a much lower lateral rate than that estimated by the manufacturer, this being 5.88 MN/m at 254 mm reference height. 2. Stiffnesses derived from component testing were lower by approximately 10% than those from whole vehicle tests; this may be partially explained...
Author(s): Chappell T.A.
Organisation(s): British Rail Research ;
1974