Welding of improved rail steel cast 3826 (TN-FM-044)

Last updated on 22 November 2013 2:33
Welding Trials have been carried out on rails manufactured from Cast 3826 Improved Rail Steel (1% Silicon). Although flash-welding and metal-arc overlaying gave promising results in the tests described, SkV thermit-welds in this rail gave some indications of inferior fatigue properties to SkV and SmW welds in BS11 rail (as...
Author(s): Ashton M.E.;Cannon D.F.;Hearne M.C.
Organisation(s): British Rail Research ;
1973
United Kingdom