Instrumentation for M.T.S dynamic fracture toughness (12.6.74) (IM-IS-213)

Last updated on 24 July 2014 3:52
Notched specimens previously cooled in a refrigerator were loaded to failure by the hydraulic ran of the MTS 'B' machine. The hydraulic ran was mounted in an 'A' frame to give a three point loading to the specimen. The specimens were cooled to -25° C and allowed to warm...
Author(s): Baker J.S.
Organisation(s): British Rail Research ;
1974